Ecogreen Technical Data

 
Physical-Mechanical
Units
Typical Value
Test method
Specific Weight
-
1.19
ASTM D 792
Tensile Strength
psi
10.500
ASTM D 638
Elongation at Rupture
%
5.0
ASTM D 638
Modulus of Elasticity
psi
384,000
ASTM D 798
Impact Resistance IZOD
ASTM D 256
Rockwell Hardness
M 90-95
ASTM D 785
Shrinkage
%
1.0
ASTM D 4802
Thermal Properties
Units
Typical Value
Test Method
Maximum Recommended
80
Continuous Service Temp
176
Deflection Temperature
93
ASTM D 648
Under Load (264psi)
199
Forming Temperature
175-180
Plastiglass
347-356
Performance
Units
Typical Value
Test Method
Outdoor Warranty
Years
8 (Clear)
ASTM D 2565/Plastic
Water Absorption (24 hrs)
%
0.30%
ASTM D 570
Flammability
-
HB
UL 94

Collapsible content

Weight of Acrylic Info

Thickness Pounds per Square Foot Thickness Pounds per Square Foot
.060" .35 1.00" 6.00
.090" .52 1.25" 7.50
.100" .57 1.50" 9.0
.118" .70 2.00" 12.0
.177" 1.10 2.50" 15.0
.220"  1.35 3.00" 18.0
.236" 1.44 3.50" 21.0
.375" 2.37 4.00" 24.0
.500" 3.00 6.00" 36.0
.750" 4.50

We are proud to carry Ecogreen® a 100% recycled and recyclable acrylic sheet. Click the banner below to learn more!